Monel Alloy Steel Strips

›

‹

›

Monel Alloy Steel Strips

Monel alloy steel strip are Monel alloy (such as Monel 400, Monel K-500, etc.) through cold rolling, hot rolling and other processing processes made of strip and plate materials. These alloys have unique physical and chemical properties and are commonly used in the manufacture of structural components and equipment requiring high corrosion resistance, high temperature resistance, and high strength. Monel alloy steel strip and steel plate with its excellent corrosion resistance, high temperature resistance, good mechanical properties and welding properties, widely used in Marine, chemical, petroleum, aerospace and other high-end industrial fields. They are suitable for a variety of harsh working environments, and can effectively cope with high temperatures, strong acids, chlorides and other corrosion
Tel:+86 15095033881
WhatsApp:+86 15095033881
Email:zhang@tntgsteel.com

// Product  Description //


ItemMonel 400 Alloy Strip and PlateMonel K-500 Alloy Strip and Plate
Main Composition

Nickel (Ni): 63%~70%Copper 

 (Cu): 28%~34%Iron 

 (Fe): ≤2.5%Manganese  

(Mn): ≤1.5%Carbon 

 (C): ≤0.30%Silicon  

(Si): ≤0.50%

Nickel (Ni): 63%~70%Copper  

(Cu): 28%~34%Aluminum 

 (Al): 2.3%~3.15%Iron  

(Fe): 1.5%~2.5%Manganese 

 (Mn): ≤1%Titanium  

(Ti): 0.35%~0.85%

Density8.8 g/cm³8.8 g/cm³
Tensile Strength550~760 MPa1035 MPa
Yield Strength240 MPa690 MPa
DuctilityExcellent, good ductility (~45%)

Lower, higher strength, 

 suitable for high-stress environments

HardnessRockwell B 85~95Rockwell C 35~45
Melting Point1300°C ~ 1350°C1300°C ~ 1350°C
Corrosion Resistance

Excellent, especially resistant to seawater, 

 acidic environments, chlorides, sulfuric acid, etc.

Outstanding, especially in high-strength  

and highly corrosive environments

High-Temperature PerformanceGood, suitable for environments up to 1000°CExcellent, especially suitable for high-temperature and high-stress environments
Machinability

Easy to machine, good cold and hot working properties,

  can be cut, stamped, bent, etc.

More difficult to machine, 

 but offers good strength and hardness, 

suitable for high-stress applications

Weldability

Good, commonly used methods include  TIG, 

 MIG, and argon arc welding

Good, commonly used methods include TIG, MIG, 

 and argon arc welding, 

 but care must be taken  

with heat input during welding

Surface TreatmentPickling, wire drawing, polishing, etc.Pickling, wire drawing, polishing, etc.
Applications

Marine engineering, chemical industry, oil & gas, 

 power, aerospace, food processing, etc.

Oil & gas, chemical industry, aerospace, 

 nuclear power, marine engineering, etc.

Common Specifications

- Thickness: 0.1 mm ~ 100 mm- 

 Width: 10 mm ~ 2500 mm-  

Length: Custom

- Thickness: 0.1 mm ~ 100 mm- 

 Width: 10 mm ~ 2500 mm-  

Length: Custom



Strip Steel.jpg


// Service Support //

Professional Service

An enterprise specializing in the production and sale of special steel, alloy steel and other high-performance steels

Quality Assurance

100% virgin material Strict quality control by inproduction 100% check and test

60a2a3334d582ad263462164d1b7daf47be7db2d4f8e0-laIurR

Good After-Sales Service

Our professional technical team can effectively help answer technical questions in product use

Customized Products

Provide customized steel product development services according to customers' specific requirements

// Request a Free Estimate //

  • Nickel-Cerium Alloy
  • Hastelloy Alloys
  • Precision Alloys
  • Nickel-Based Alloys
  • Monel Alloy
  • High-Temperature Alloys
  • Metal Powders
Submit

// Transport Packaging //

  • 6a225df06cd541579907a237014053f4
  • 微信图片_20210412160315-31
  • wKj0iWAc50-AS-9-AAJuI7gQcS0026
  • 16454c4a3c86314d296ec98747595860
  • 704a4c816c49d3a3027acf1a2e11d23
  • 微信图片_20220407115052
  • 78307ccb9551295a13bb730cb5e9af5f
  • 微信图片_2025-09-10_153633_235

// Products Recommended //

 Our products include corrosion-resistant alloys, high-temperature alloys, precision alloys, Hastelloy alloys, Monel alloys, INCONEL, INCOLOY, copper nickel alloys, titanium and titanium alloys, zirconium and zirconium alloys, nickel and nickel based alloys, nickel cobalt based heat-resistant alloys, hafnium alloys, and more than 60 other alloy materials.

GET IN TOUCH