Cobalt-Based Superalloy Powders (Stellite Series)

›

‹

›

Cobalt-Based Superalloy Powders (Stellite Series)

(Outstanding anti-fretting, anti-galling, thermal wear & hot corrosion resistance up to 900~1100°C)
Tel:+86 15095033881
WhatsApp:+86 15095033881
Email:zhang@tntgsteel.com

// Product  Description //

(Outstanding anti-fretting, anti-galling, thermal wear & hot corrosion resistance up to 900~1100°C)

Grade

Hardness

Key Advantages

Application Scenarios

Stellite 6

HRC40~45

Balanced toughness & wear resistance, most universal cobalt-based powder

High-temperature valve sealing faces, engine exhaust valves, turbine shafts, pump impellers, hardfacing for rolling mills, cavitation erosion repair

Stellite 12

HRC48~52

Higher carbide content, superior abrasion resistance

Mud valves, screw conveyors, high-temperature shear blades

Stellite 1

HRC54~58

Ultra-high hardness & abrasion resistance

High-pressure valve seats, cutting edges, wire drawing die liners

Stellite 21

Excellent cavitation & seawater corrosion resistance

Hardfacing for hydro-turbine blades & marine propellers against cavitation erosion


Other Cobalt Grades

· Haynes 188, GH5188: High-temperature oxidation resistant, for aero-engine combustion chambers & heat shields

Stellite 6K: High-carbon modified grade for heavy-load wear cladding service


// Service Support //

Professional Service

An enterprise specializing in the production and sale of special steel, alloy steel and other high-performance steels

Quality Assurance

100% virgin material Strict quality control by inproduction 100% check and test

60a2a3334d582ad263462164d1b7daf47be7db2d4f8e0-laIurR

Good After-Sales Service

Our professional technical team can effectively help answer technical questions in product use

Customized Products

Provide customized steel product development services according to customers' specific requirements

// Request a Free Estimate //

  • Nickel-Cerium Alloy
  • Hastelloy Alloys
  • Precision Alloys
  • Nickel-Based Alloys
  • Monel Alloy
  • High-Temperature Alloys
  • Metal Powders
Submit

// Transport Packaging //

  • 6a225df06cd541579907a237014053f4
  • 微信图片_20210412160315-31
  • wKj0iWAc50-AS-9-AAJuI7gQcS0026
  • 16454c4a3c86314d296ec98747595860
  • 704a4c816c49d3a3027acf1a2e11d23
  • 微信图片_20220407115052
  • 78307ccb9551295a13bb730cb5e9af5f
  • 微信图片_2025-09-10_153633_235